张伟,王志群.残余应力下厚壁筒表面裂纹的应力强度因子计算[J].计算力学学报,2000,17(3):360~364 |
| 码上扫一扫! |
残余应力下厚壁筒表面裂纹的应力强度因子计算 |
Calculation of stress intensity factor about a thick-walled cylinder with an surface crack under autofrettage stresses |
修订日期:1998-11-04 |
DOI:10.7511/jslx20003065 |
中文关键词: 应力强度因子 厚壁筒 结构 裂纹 残余应力 |
英文关键词:stress intensity factor,thick\|walled cylinder,structure,crack |
基金项目: |
张伟 王志群 |
[1]上海交通大学船舶与海洋工程学院 [2]南京理工大学应用力学系 |
摘要点击次数: 1252 |
全文下载次数: 8 |
中文摘要: |
本文首先介绍了边界元法计算裂纹尖端应力强度因子的基本理论,接着利用边界元法计算了在残余应力下不同厚壁筒内表面椭圆裂纹的应力强度因子,研究了其大不随椭圆裂纹不同而变化的规律,为厚壁筒结构的设计,制造以及疲劳寿命分析提供了许多有价值的参考资料。 |
英文摘要: |
HT5SS]In this paper, first, the basic theories of calculating stress intensity factor at a crack\|tip by FEM are provided. Then, the stress intensity factors are calculated about thick\|walled cylinders with various crack size internal semi\|elliptical surface crack under autofrettage residual stresses and its change laws are studied. These researches in this paper are very valuable to design, making and fatigue analysis about thick\|walled cylinder structure. |
查看全文 查看/发表评论 下载PDF阅读器 |